Relay Welding Process and Cleaning Process
In this article, MEISHUO will introduce the RELAY welding process and cleaning process.
Coating Flux
PCB type non plastic relay is easy to be polluted by flux. It is suggested to use anti flux or plastic relay to prevent flux gas from invading the gap between the lead end of the base and the shell. If the anti flux relay is preheated and dried (100℃ for 1 minute), it can further prevent flux from invading.
Welding Process
When using flux coating or automatic welding, care should be taken not to damage the relay performance. Flux resistant relay or plastic encapsulated relay can be used for immersion welding or wave soldering process, but the maximum welding temperature and time should be controlled according to the selected relay.
a. Wave Soldering: the recommended soldering temperature is 240℃~ 260℃, the time is about 5 seconds, and the best soldering temperature is 250℃. For other welding temperatures and welding times (for example, higher solder temperatures will shorten the tin dipping time), please contact our technical service support or confirm the welding quality.
b. Manual Welding: the recommended welding temperature is 300℃ - 350℃, and the welding time is controlled within 2 seconds.
c. Cooling: the heating of the relay caused by the soldering process can be alleviated by cooling in the process, so do not change the temperature suddenly, especially to avoid cold shock to the thermal relay.
Cleaning Process
Clean free flux shall be used for welding as far as possible, and integral cleaning of the relay shall be avoided. Prevent the detergent from entering the relay and causing failure. It is forbidden to use ultrasonic cleaning to avoid contact with cold welding, enameled wire breakage, and other structural damage caused by ultrasonic energy. After cleaning and drying, ventilation should be carried out immediately to reduce the relay to room temperature.
Apply Preservative
Sometimes, in order to ensure the moisture resistance and high insulation of the circuit board, it is necessary to coat the circuit board with preservatives. The soft adhesive without silicon should be selected. The coating process should avoid the negative pressure generated by the relay and the inhalation of preservatives.
- |
- +1 赞 0
- 收藏
- 评论 0
本文由上山打老虎转载自MEISHUO News,原文标题为:RELAY WELDING PROCESS AND CLEANING PROCESS,本站所有转载文章系出于传递更多信息之目的,且明确注明来源,不希望被转载的媒体或个人可与我们联系,我们将立即进行删除处理。
相关推荐
Maintenance Method of Automobile Relay
In this article MEISHUO will introduce the maintenance method of automobile relay.
设计经验 发布时间 : 2023-12-03
Automotive Relay Storage Environment
MEISHUO will introduce the automotive relay storage environment in this article.
设计经验 发布时间 : 2023-12-04
Selection Guide for Automotive Relays
When selecting automotive relays, analysis and research can be carried out item by item according to the following points: shape and installation method, input parameters, output parameters, environmental conditions, electromagnetic compatibility, installation and use requirements.
器件选型 发布时间 : 2023-12-06
美硕(MEISHUO)继电器选型指南
描述- 浙江美硕电气科技股份有限公司是一家专业研发、生产及销售继电器、电动水阀等产品的高新技术企业,产品广泛应用于家用电器、汽车电子、工业控制、电力电子、智能家居等领域。
型号- MPD,MPF,ME106,MPE,ME105,MPH,ME100,MPJ,MPI,ME101,MPL,MCA-S-112-C1H,MPN,MPM,MPP,MPI-S-112-C-1NF-01,ME112-1A-20-QLT,MPR,MPT,ML103-S-112-A-L1-F,MPX,MPZ,MPY,MAB-S-112-A-1YR,MLE-80-112-A-L1-XXX,MPQ1-S-112D-A-6-01,ME115,ME114,ME117,ME116,ME112,MALC,MALA,MPM-212D-C1D,MAA,MPE-S-112-A-NF,MAC,MPL-1-12-A-TF,MPQ1 40A,MAB,MPDN-S-112-AF,MAD,MLQ-60112-AL1-RXXX,MLM-120,ME101-120,MAA-S-112-C-R,MALN,MAH,ML100-S-112-A-L2,ME100-S1A-XF,MPD-S-112-A,MPF-S-1-12-A-2F,ME101-200-1A-1-F,ME108,MAS,MAR,ME109,MALC-S-112-A-L1-R1,ME118-1A-1-F,ME100-S-1A-XF,ME115-1A-1-F,MAH-S-112-C-1R,MPDN,MLQ-100,ML601-S-1A-L1-RFXXX,MPQ4-S-112D-A-L,MPL-S-112-A-T-F,MCB-S-212-C-M,MPQ4-S-112D-A-T,MAH3,MLQ-100112-AL1-RXXX,MA101-S-112-2A,MLH-200212-AL1-RXXX,ME101-140-1A-1-F,MLC-100-212-A-L1-R-XXX,MCA,MPX-S-112-A-T-F,MLQ-60,MCB,MCD,ME101-140,MPZ-S-212-A-T,MAH3-S-112-C-1R,MA101,MLL-120312-AL1-RXXX,MLE,MLH,ML101-S-112-A-L2,MLG,MLQ-90,MLK,MLM-120112-AL1-RXXX,MLN,ME105-1A-1-F,MLP-120112-AL1-RXXX,MLP,ML100,ML101,ML102,ML103,MPA-S-112-A,MPD-16,ME114-1AB-F,MLC-100,ME101-120-1A-1-F,MPQ2-S-112D-C,MLK-60112-AL1-RXXX,MALA-S-112-A-X,MALN-S-112-A-L1-R-1,ME101-1A-1-F,MALN-S-112-A-L1--R-1,MAR-S-112-A-R,ME101-200,MPY-S-112-A-P,ME101-1A-A-F,MLQ-90112-AL1-RXXX,MPQ2,ME117-1A-1-F,MPQ4,MPN-112D-C1D,MAC-S-212-C-P,ME116-1A-1-F,MPQ1,ME108-2A-1B-F,MLG-100312-AL1-RXXX,MPT-224D-A-FL-F,MPH-S-1-12-C-1F,MPQ4-L,ML601,MAD-S-112-C,MLL-120,ME118,ME106-S-1A-P1-F,MAS-S-112-A-R,MPL-H,MLN-90312-AL1-RXXX,ME109-S-1A-HYF,MPJ-S-112-A-1NF,ML102-S-112-A-L1-R-F,MPR-S-112-A,MCD-S-112-A-11F,MPB,MPA
MEISHUO High Power Electromagnetic Relay MLQ-100-209-B-L1 with a Max. Switching Voltage of 250VAC
Electromagnetic relay is an electronic control device. It has a control system and a controlled system. It is usually used in automatic control circuits. In fact, it uses a smaller current and a lower voltage to control a larger current. A kind of “automatic switch“ for higher voltage. Therefore, it plays the role of automatic adjustment, safety protection, and conversion circuit in the circuit.
产品 发布时间 : 2024-04-29
电子商城
现货市场
服务
可加工PCB层数:1-30层;板材类型:FR4板/铝基板/铜基板/刚扰结合板/FPC板/高精密板/Rogers高频板;成品尺寸:5*5mm~53*84cm;板厚:0.1~5.0mm。
最小起订量: 1 提交需求>
可贴片样板PCB尺寸范围50*50~910*600mm,设备贴装最小元件尺寸:01005,设备贴装最小pitch(IC类)元件:0.15mm;设备贴装最小pitch(BGA类)元件:0.2mm。
最小起订量: 1pcs 提交需求>
登录 | 立即注册
提交评论